  • 2-3(1713941975908).png

NC30Fe forgings

For any temperature and concentration of hydrochloric acid has excellent corrosion resistance. At the same time, it has good corrosion resistance to sulfuric acid, acetic acid, formic acid, phosphoric acid and other non-oxidizing media.

Classification:

Product Display

Key words: nickel-based alloy material

Message
  • DESCRIPTION

    Overview

    NC30Fe is an austenitic stainless steel product. According to GB/T20878-2007, stainless steel is defined as steel with stainless and corrosion resistance as its main characteristics, and a chromium content of at least 10.5% and a carbon content of no more than 1.2%.

    NC30Fe

    Chemical composition

    Ni C Cr Fe Si Mn
    ≥58 ≤0.05 27.00~30.0 07.0~1 1.0 ≤0.05
    S Cu P
    ≤0.05 ≤0.015 ≤0.54.

A nickel-chromium-molybdenum alloy with the addition of niobium, which acts with molybdenum to harden the alloy matrix, thereby exhibiting high strength properties without heat treatment. The alloy is resistant to various harsh corrosive environments, especially pitting and crevice corrosion. It is used in chemical, aviation and marine engineering, pollution control equipment, and nuclear reactors.

 

The low carbon alloy 625 after softening annealing is widely used in the chemical process industry, and its good corrosion resistance and high strength make it can be used as a thin structural component. 625 alloys can be applied in contact with seawater and subjected to high mechanical stress. Typical application areas:
1. Components of organic chemical processes containing chlorides, especially where acid chloride catalysts are used;
2. For the manufacture of digesters and bleaching ponds for the pulp and paper industry;

3. The absorption tower, reheater, flue gas inlet baffle, fan (wet), agitator, deflector and flue in the flue gas desulfurization system;

4. For the manufacture of equipment and components used in acid gas environments;
5. Acetic acid and acetic anhydride reaction generator;
6. Sulfuric acid condenser.