- DESCRIPTION
-
Overview
Nickel-chromium alloy, which can be precipitation hardened by adding aluminum and titanium. The alloy has good oxidation resistance and still has high tensile strength and creep rupture properties at 815℃. Used for gas turbine components, bolts, nuclear steam generator pipe brackets and internal combustion engine exhaust valves

Chemical composition
C≤0.10 wt. %; Cr: 18.0~21.0 wt. %; Si≤1.0 wt. %; Co≤0.20 wt. %; Ti:1.8~2.7 wt. %;Al:1.0~1.8 wt. %; B≤0.0080 wt. %; S≤0.015 wt. %; Ni: (balance)
Application
It has good strength and very excellent corrosion resistance and oxidation resistance at high temperatures. These advantages make the alloy widely used in high-temperature hot forging parts such as aviation, aerospace, power stations and transportation.
Nimonic80A forgings are a high-end industrial material with excellent performance.
Its main features include:
High strength: able to withstand huge pressure and load, ensuring structural stability in various harsh environments.
High temperature resistance: still maintain good mechanical properties under high temperature conditions, suitable for high temperature working scenes.
Good corrosion resistance: effectively resist the erosion of various corrosive media and extend the service life.
Excellent processing performance: convenient for various processing processes such as forging, and can shape forgings of various shapes and sizes according to specific needs.
Nimonic80A forgings are widely used in the aerospace field to manufacture key components, such as engine components, etc., to ensure the high performance and reliability of aircraft. At the same time, they also play an important role in the energy, chemical and other industries, and are used to manufacture high temperature and high pressure resistant equipment components.
A nickel-chromium-molybdenum alloy with the addition of niobium, which acts with molybdenum to harden the alloy matrix, thereby exhibiting high strength properties without heat treatment. The alloy is resistant to various harsh corrosive environments, especially pitting and crevice corrosion. It is used in chemical, aviation and marine engineering, pollution control equipment, and nuclear reactors.
The low carbon alloy 625 after softening annealing is widely used in the chemical process industry, and its good corrosion resistance and high strength make it can be used as a thin structural component. 625 alloys can be applied in contact with seawater and subjected to high mechanical stress. Typical application areas:
1. Components of organic chemical processes containing chlorides, especially where acid chloride catalysts are used;
2. For the manufacture of digesters and bleaching ponds for the pulp and paper industry;
3. The absorption tower, reheater, flue gas inlet baffle, fan (wet), agitator, deflector and flue in the flue gas desulfurization system;
4. For the manufacture of equipment and components used in acid gas environments;
5. Acetic acid and acetic anhydride reaction generator;
6. Sulfuric acid condenser.